I can help on this one...
Just had the bottom soda blasted in OCT before she went into storage. Ran about $1200 for a 36'. Nice job removing the old paint, yet leaving the gel coat with a nice surface for reapplication. Made my life a lot easier than scraping and sanding. I have some pic's that I can share if interested. Just ask.
One thing to watch for... they did a great job draping the boat to contain the mess, but neglected to mask at the waterline. Result was some overspray north of the line, which I had to sand/buff back down to a shine. It was either that or move the water line paint north to cover.
Next step was to locate, grind any stress cracks and open any blisters. You get pretty intimate with your hull after laying under there feeling for any raised areas, and testing them with a small ball hammer (sound changes at any blisters - trick I learned on B-ed). Done with all that now. Leaving her dry out for 4 to 6 weeks before refilling (found a couple wet ones), and then plan to barrier coat in April.